MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
BYK ADD-VANCE® SA 420 Slip/anti-block additive  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fields of application: Improves slip and anti-block properties of thermoplastics. It can also be used as a release agent for injection molded products.
Examples: (L)LDPE, HDPE, PP, PS, HIPS, TPO, ABS and other thermoplastics which are processed in films, sheets, profiles, injection molded products, etc.

Mode of action and advantages: ADD-VANCE SA 420 provides slip and anti-block properties. ADD-VANCE SA 420 reduces friction between two surfaces for instance between polymer and metal. As a consequence the slip properties of the product are improved

Advantages: Excellent anti-block properties, already at low dosing rates; Excellent organoleptic properties; Good printability; Non-toxic and non-corrosive; Injection molding: also improved demoulding and product release; Non-sticking pellets, dust free dosing; and Safe and easy handling

Regulations: ADD-VANCE SA 420 is suitable for food packaging products as the active ingredients are in compliance with current food contact regulations.

Former ADDCOMP product line, acquired by BYK.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 220 °C
 
Descriptive Properties
AppearanceWhite to off-white granules
Dosing Level0.3-1%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPADDC25 / 133238

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.