MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vicone High Performance Rubber VicoSeal™ 617N-BK Rubber Vulcanized to SS304
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Two Material Product:
Material 1: VicoSeal™ 617N-70 DURO
Material 2: SS304 nitrile vulcanized to SS304 (RoHS Approved)

Property data reported for 617N.

Information provided by Vicone

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.219 g/ccASTM D3165
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 69ASTM D2240
 75.97
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aging; ASTM D573
Tensile Strength, Yield 16.8 MPaASTM D412
 15.792 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aging; ASTM D573
Elongation at Break 433.6 %ASTM D412
 305.86 %
@Treatment Temp. 100 °C,
Time 252000 sec
Heat Aging; ASTM D573
Compressive Modulus 0.590 MPa
@Strain 5.0 %
 1.01 MPa
@Strain 10 %
 1.59 MPa
@Strain 20 %
 2.10 MPa
@Strain 25 %
Compression Set 6.44 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Vicone High Performance Rubber VicoSeal™ 106C-BK High Performance EPDM Rubber
Vicone High Performance Rubber VicoSeal™ 07EK-BK High Performance EPDM Rubber
Vicone High Performance Rubber VicoSeal™ 003R-BK Rubber Vulcanized to Steel
Chemours Viton® GF-600S with 5-MT Black Fluoroelastomer Compound

PAVICON9A2 / 130895

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.