MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ MG94 ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Superior flow, injection molding ABS. Good impact. For thin-wall applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Moisture Absorption 0.160 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
Melt Flow 39 g/10 min
@Load 10.0 kg,
Temperature 220 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 129ISO 2039-2
Ball Indentation Hardness 95.0 MPaISO 2039-1
Tensile Strength at Break 35.0 MPa5 mm/min; ISO 527
 35.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 40.0 MPa5 mm/min; ISO 527
 46.0 MPa50 mm/min; ISO 527
Elongation at Break 35 %5 mm/min; ISO 527
 45 %50 mm/min; ISO 527
Elongation at Yield 2.0 %5 mm/min; ISO 527
 2.3 %50 mm/min; ISO 527
Tensile Modulus 2450 MPa1mm/min; ISO 527
Flexural Yield Strength 65.0 MPa2 mm/min; ISO 178
Flexural Modulus 2500 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 23.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 87.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 87.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 99.0 °CRate B/50; ISO 306
 100 °CRate B/120; ISO 306
Glow Wire Test 650 °C
@Thickness 3.20 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 210 - 250 °CInjection Molding
Zone 1 200 - 240 °C
Zone 2 220 - 260 °C
Zone 3 220 - 260 °C
Melt Temperature 220 - 260 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 85.0 - 95.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10108 / 243575

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.