MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Pyrotek Ceramite® CSR-S Refractory
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Ceramite® CSA and CSR series are precast refractory materials based on silicon carbide. Used in areas of heavy wear in the aluminium industry, they have high abrasion resistance and high thermal conductivity. Different aggregates in each formulation determine the properties for each product. Ceramite CSA and CSR series are high performance refractories for high temperature applications.

Benefits:

  • Good strength
  • Good wear resistance
  • Good chemical resistance
  • High thermal conductivity
  • High thermal shock resistance
  • Alkali resistance

Information provided by Pyrotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
@Temperature 600 °C
 2.80 g/cc
@Temperature 20.0 °C
Grain Size <= 3000 µm
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0120 GPa
@Temperature 20.0 °C
Cold
 0.0180 GPa
@Temperature 600 °C
Cold
 0.0180 GPa
@Temperature 850 °C
Cold
 0.0200 GPa
@Temperature 1000 °C
Cold
 0.0280 GPa
@Temperature 1000 °C
Hot
Compressive Strength 120 MPa
@Temperature 850 °C
Cold
 122 MPa
@Temperature 1000 °C
Cold
 131 MPa
@Temperature 20.0 °C
Cold
 205 MPa
@Temperature 600 °C
Cold
Abrasion 0.80
@Temperature 20.0 °C
[cm^3]
 0.90
@Temperature 600 °C
[cm^3]
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1000 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Pyrocast L-40 Insulating Refractory
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrotek Pyrocast 80 Lightweight Castable Refractory
Pyrotek Pyrocast HD Castable Refractory
Pyrotek Pyrocast AR70 Low-Density Refractory Castable

CPYRO517 / 199539

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.