MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M 7710 Acetate Identification Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Label Material 7710 gloss clear acetate with 3M™ 400 high tack acrylic adhesive offers consistent, high quality appearance and excellent UV resistance. The transparent film easily die-cuts which helps extend die life in comparison with polyester label stocks. When used as an overlaminate, it provides depth, protection and rigidity as well as enhancing the appearance of the underlying label.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.800 milAdhesive
 2.50 milLiner
 3.00 milFacestock
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 1.50 pliPolypropylene, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 1.50 pliPolypropylene, 180° Peel, Conditioned for 3 days at 66°C; ASTM D3330
 1.5625 pliStainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 1.875 pliPolypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.5625 pliStainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.625 pliABS, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
 2.75 pliABS, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 3.00 pliABS, 180° Peel, Conditioned for 3 days at 66°C; ASTM D3330
 3.125 pliStainless Steel, 180° Peel, Conditioned for 3 days at 66°C; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 77.0 °C
Minimum Service Temperature, Air -26.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= -12.0 °CApplication
Shelf Life 24.0 Month
 
Descriptive Properties
Adhesive Type400 high tack acrylic
Liner43# densified kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33447 / 168194

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.