MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Entec HYBOOST® 402 Masterbatch, LLDPE
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: HyBoost-402 is a finely dispersed TiO2 with filler to reduce cost in a prime LLDPE carrier resin for ease of incorporation into final product. HyBoost-402 is designed for higher end applications such as graphic film.
Description: Masterbatch White concentrate based on LLDPE with 70% TiO2 blend.
Applications: HyBoost-402 is carefully dispersed into an LLDPE carrier for use in many critical applications where dispersion is important. These applications may include thin gauge film, blow molded articles, sheet extrusion and injection molding. HyBoost-402 white utilizes an FDA compliant resin and pigments.

Availability: North America

Agency Ratings: FDA Food Contact

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Additive Concentration0.7
Additives CategoryMasterbatch -- Pigment -- White
Carrier ResinPolyethylene or ethylene-olefin copolymer (PE)
Chemical DescriptionTiO2
White Pigment CompositionTitanium Dioxid (TiO2)0.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENTB707 / 311400

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.