MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Eastman 11 Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: This product is used in laminate film.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccASTM D1505
Water Vapor Transmission 6.00 g/m²/dayASTM F372
Oxygen Transmission 10.0 cc-mm/m²-24hr-atmASTM D3985
Carbon Dioxide Transmission 49.0 cc-mm/m²-24hr-atmASTM D1434
Viscosity Measurement 0.70Inherent; EMN-A-AC-G-V-1
Thickness 254 micronsASTM D374
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 52.0 MPaASTM D882
Film Tensile Strength at Yield, TD 52.0 MPaASTM D882
Film Elongation at Break, MD 400 %ASTM D882
Film Elongation at Break, TD 400 %ASTM D882
Film Elongation at Yield, MD 4.0 %ASTM D882
Film Elongation at Yield, TD 4.0 %ASTM D882
Tensile Modulus 1.90 GPaTD; ASTM D882
 1.90 GPaMD; ASTM D882
Tear Strength, Total 9.10 NSplit Tear Method, 254mm/min, MD; ASTM D1938
 9.10 NSplit Tear Method, 254mm/min, TD; ASTM D1938
 93.0 NPPT Tear Resistance, MD; ASTM D2582
 93.0 NPPT Tear Resistance, TD; ASTM D2582
Tear Strength 36.0 kN/mTrouser Tear Resistance, MD; ISO 6383-1
 36.0 kN/mTrouser Tear Resistance, TD; ISO 6383-1
Elmendorf Tear Strength, MD 13.7 g/micronASTM D1922
Elmendorf Tear Strength, TD 16.7 g/micronASTM D1922
Dart Drop 1.57 g/micron23°C; ASTM D1709
 1.97 g/micronat -18°C; ASTM D1709
Film Tensile Strength at Break, MD 59.0 MPaASTM D882
Film Tensile Strength at Break, TD 55.0 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 0.80 %ASTM D1003
Gloss 108 %at 45°; ASTM D2457
Transmission, Visible 85 %Transparency; ASTM D1746
 89 %Regular Transmittance; ASTM D1003
 91 %Total Transmittance; ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PE9062 / 35118

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.