MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Sintox™ AL Technical Ceramic
Categories: Ceramic

Material Notes: High purity porous alumina ceramic, used extensively for long-life laser reflectors. This material is sintered at high temperatures to achieve a controlled porosity.

Applications:

  • Pumping chambers for flash lamp and continuous wave lasers using media such as Nd:YAG lasers, Alexendrite — low to high power, single or multiple lamp designs used for welding, cutting, marking and in medical lasers
  • Layered and segmented pumping chambers for diode pumped lasers
  • Intense Pulse Light (IPL) applications for cosmetic surgery

information provided by Morgan Advanced Materials

Key Words: Technical Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.20 g/cc
Porosity 20 %apparent, nominal
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 150 MPa3 point; ASTM C1161
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.90 µm/m-°C
@Temperature 200 - 500 °C
 9.00 µm/m-°C
@Temperature 200 - 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99.7 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill® TPX-PBT-98010 BN069
Overview of materials for Thermoset Polyester Glass and Mineral Filled BMC
Aluminum, Al

CMORF8034 / 203511

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.