MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC PPE reactive chemistries SA9000
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: NORYL™ SA9000 resin is a modified, low molecular weight, bi-functional oligomer based on polyphenylene ether (PPE) with vinyl end-groups. It is well suited for use with other unsaturated monomers and resins which cure via free radical reactions. These include styrenic, allylic, acrylic, maleimide, methacrylic, and unsaturated polyesters monomers and resins. It has a low solution viscosity and outstanding solubility in toluene & methyl ethyl ketone (MEK). Key application areas are in electronic packaging which include PCB laminates, copper clad laminates, non-epoxy prepregs, and adhesives. The use of NORYL SA9000 is especially advantageous in insulating materials where very low dielectric properties and decreased moisture absorption are required.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccASTM D792
Solubility 500000 ppmSolubility, Methyl Ethyl Ketone (21°C); SABIC method
 500000 ppmSolubility, Toluene (21°C); SABIC method
Viscosity 160 cP50 wt% in methyl ethyl ketone, 25°C; SABIC method
 298 cP50 wt% in toluene, 25°C; SABIC method
Viscosity Measurement 0.090dl/g; SABIC method
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.54
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.00070
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 160 °Chalf width; SABIC method
 
Descriptive Properties
Mn2300SABIC method
Phenolic End-group Content-300 ppmSABIC method
Physical FormPOWDERSABIC method
Vinyl Functionality1.9SABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80009 / 287956

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.