System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
AISI 1117 Steel, cold drawn, high temperature, stress relieved, round
Categories:
Metal
;
Ferrous Metal
;
Carbon Steel
;
AISI 1000 Series Steel
;
Low Carbon Steel
Material Notes:
Applications include medium duty shafts, studs, pins, distributor cams, cam shafts, and universal joints.
Key Words:
UNS G11170, ASTM A29, ASTM A107, ASTM A108, FED QQ-S-637 (C1117), MIL SPEC MIL-S-18411, SAE J403, SAE J412, SAE J414
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
7.87
g/cc
Typical for steel.
Mechanical Properties
Original Value
Comments
Hardness, Brinell
111
@Diameter 50.8 - 76.2 mm
121
@Diameter 31.8 - 50.8 mm
131
@Diameter 22.2 - 31.8 mm
143
@Diameter 15.9 - 22.2 mm
Hardness, Knoop
129
@Diameter 50.8 - 76.2 mm
Converted from Brinell
140
@Diameter 31.8 - 50.8 mm
Converted from Brinell
150
@Diameter 22.2 - 31.8 mm
Converted from Brinell
163
@Diameter 15.9 - 22.2 mm
Converted from Brinell
Hardness, Rockwell B
64
@Diameter 50.8 - 76.2 mm
Converted from Brinell
68
@Diameter 31.8 - 50.8 mm
Converted from Brinell
73
@Diameter 22.2 - 31.8 mm
Converted from Brinell
78
@Diameter 15.9 - 22.2 mm
Converted from Brinell
Hardness, Vickers
115
@Diameter 50.8 - 76.2 mm
Converted from Brinell
126
@Diameter 31.8 - 50.8 mm
Converted from Brinell
136
@Diameter 22.2 - 31.8 mm
Converted from Brinell
149
@Diameter 15.9 - 22.2 mm
Converted from Brinell
Tensile Strength, Ultimate
380
MPa
@Diameter 50.8 - 76.2 mm
415
MPa
@Diameter 31.8 - 50.8 mm
450
MPa
@Diameter 22.2 - 31.8 mm
485
MPa
@Diameter 15.9 - 22.2 mm
Tensile Strength, Yield
310
MPa
@Diameter 50.8 - 76.2 mm
345
MPa
@Diameter 15.9 - 22.2 mm
345
MPa
@Diameter 22.2 - 31.8 mm
345
MPa
@Diameter 31.8 - 50.8 mm
Elongation at Break
15 %
@Diameter 31.8 - 50.8 mm
in 50 mm
15 %
@Diameter 50.8 - 76.2 mm
in 50 mm
16 %
@Diameter 22.2 - 31.8 mm
in 50 mm
18 %
@Diameter 15.9 - 22.2 mm
in 50 mm
Reduction of Area
40 %
@Diameter 31.8 - 50.8 mm
40 %
@Diameter 50.8 - 76.2 mm
45 %
@Diameter 15.9 - 22.2 mm
45 %
@Diameter 22.2 - 31.8 mm
Modulus of Elasticity
200
GPa
Typical for steel
Bulk Modulus
160
GPa
Typical for steel.
Poissons Ratio
0.29
Typical For Steel
Shear Modulus
80.0
GPa
Typical for steel.
Izod Impact
81.0
J
as rolled
85.0
J
normalized at 900°C (1650°F)
94.0
J
annealed at 855°C (1575°F)
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.0000174
ohm-cm
Typical steel
Thermal Properties
Original Value
Comments
CTE, linear
11.5
µm/m-°C
@Temperature 20.0 °C
Typical steel
12.2
µm/m-°C
@Temperature 0.000 - 300 °C
Typical for steel
13.9
µm/m-°C
@Temperature 0.000 - 500 °C
Typical for steel
Specific Heat Capacity
0.481
J/g-°C
@Temperature >=100 °C
condition unknown
Thermal Conductivity
51.9
W/m-K
Typical steel
Component Elements Properties
Original Value
Comments
Carbon, C
0.14 - 0.20 %
Iron, Fe
98.33 - 98.78 %
As remainder
Manganese, Mn
1.0 - 1.3 %
Phosphorus, P
<= 0.040 %
Sulfur, S
0.080 - 0.13 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AISI 1117 Steel, cold drawn, low temperature, stress relieved, round
AISI 1117 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
AISI 1117 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round
AISI 1117 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1117 Steel, mock carburized at 925°C (1700°F) for 8 hours, 790°C (1450°F) reheat, water quenched, 175°C (350°F) temper, round
M1117N / 7140
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.