MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Indium Corp. 3541 Wave Solder Flux, No-Clean
Categories: Fluid; Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: 3541 No-Clean is a low-solids flux specially formulated to be used for wave soldering where the cleaning process has been eliminated. This flux contains a small amount of resin which enhances the wetting properties.
3541 No-Clean is activated by a multi-component, synergetic fluxing system, which improves solderability. Any post-soldering residues are considered non-corrosive.
3541 No-clean leaves a "tack-free" surface and does not interfere with ATE testing.

Features:

  • Eliminates the need for cleaning
  • Reduces solder ball formation
  • Excellent solderability on standard board finishes and alternative coating

Physical Properties

  • Color: Straw
  • J-STD-004 Flux Type: ORL0

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.800 g/cc
@Temperature 25.0 °C
 0.806 g/cc
@Temperature 15.5 °C
Solids Content 4.31 %
 
Chemical PropertiesOriginal ValueComments
Acid Value 25
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.88e+13 ohmControl - final; Standard Bellcore
 2.68e+13 ohmControl - initial; Standard Bellcore
 3.76e+9 ohm
@Time 605000 sec
Control; IPC B25A
 1.74e+10 ohm
@Time 86400 sec
Control; IPC B25A
 
Thermal PropertiesOriginal ValueComments
Flash Point 54.0 °FTCC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Solder/Braze Alloy

NNIN990 / 131629

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.