MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Struktol TPW 012 Processing Additive
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: An optimized blend of special waxes and oleo chemicals.

STRUKTOL® TPW 012 is a formulated blend of lubricants designed to provide optimum processing, surface and physical property characteristics of rigid PVC compounds. STRUKTOL® TPW 012 is recommended for wood-filled PVC and has been shown to provide significant processing and output rate benefits when compared to traditional lubricant formulations.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/cc
Additive Loading 2.0 - 8.0 %parts depending on formulation and processing needs.
 
Thermal PropertiesOriginal ValueComments
Dropping Point 122 - 128 °C
 
Descriptive Properties
AppearanceBeige to light tan pastilles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Struktol TR EBS Processing Additive, Dispersant
Struktol TR 041 Processing Additive
Struktol TPW 113 Processing Additive

PSTRUK32 / 69260

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.