MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik REWOQUAT® W 222 LM Softener
Categories: Other Engineering Material

Material Notes: Product description: Bis-(tallowacylamidoethyl)-polyethoxy-methyl-ammonium-methosulfate.

Application: REWOQUAT® W 222 LM is recommended for the preparation of yarns and the softening of fabrics made of cellulosic, synthetic or blended fibers.

Properties / Benefits: Being a strongly substantive cationic, REWOQUAT® W 222 LM can be applied by the exhaust method or from short liquor (padder, backwasher). REWOQUAT® W 222 LM is stable to hydrolysis and non-yellowing Additionally, it has antistatic and emulsifying properties. REWOQUAT® W 222 LM can easily be formulated with siloxanes, contributing to synergistic effects or performance fine tuning of the respective formulations. REWOQUAT® W 222 LM imparts to the treated goods a soft, dry and fluffy hand, being especially recommended for terry cotton.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 84 - 87 %
pH 5.0 - 6.5
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 6.0
 
Descriptive Properties
Appearancelight yellow, lardlike paste
Content7.5-9.5%IPA
 82-88%Active matter, mw=898

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIL519 / 196723

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.