MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
PolyMirae Moplen HP524J BDDP Film Grade Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Moplen HP524J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP524J is a homopolymer particularly suitable for BOPP (Tender) film. Moplen HP524J resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520.

Features: High Transparency; High Stiffness; Low film shrinkage

Applications: General purpose packaging; Lamination Film; Adhesive tape

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ASTM D785
Tensile Strength, Yield 360 kg(f)/cm²ASTM D638
Elongation at Yield 12 %ASTM D638
Flexural Modulus 15500 kg(f)/cm²ASTM D790
Izod Impact, Notched 5.00 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °CASTM D648
Vicat Softening Point 153 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 6D20 Polypropylene Random Copolymer Resin
Buckeye Polymers BP RPPC 0510 Blk Reprocessed Polypropylene, Unfilled
Braskem H 504 XP Bioriented Film Polypropylene
Borealis HC401BF Polypropylene Homopolymer
Borealis BE961MO Polypropylene for Injection Molding

PMIRAE36 / 53148

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.