MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sika Level-01 Primer Concrete primer and sealer
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Sika® Level-01 Primer is a one-part, water-dispersed and solvent-free, acrylic-based solution used to prime and seal floor surfaces prior to the application of the Sika® Level products.

Where to Use: Use as a primer/sealer for absorbent substrates including concrete and cement screeds. Particularly suitable as an adhesion promoter and surface sealer beneath Sika® Level product range, enhancing the bond and integrity of the underlayment when applied onto porous substrates.

Advantages:

  • Ready to use, no dilution required.
  • Water-based and solvent-free.
  • Penetrates substrate to reduce outgassing and formation of bubbles in the underlayment.
  • Prevents water loss from the underlayment into the substrate.
  • Quick-drying and fast film formation to increase productivity.
  • Achieves excellent bond values throughout the recommended range of application temperatures.
  • Effectively seals concrete surfaces in a single, economic operation.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/cc
Solids Content 23 %
Volatile Organic Compounds (VOC) Content <= 10 g/lEPA method 24
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength >= 217 psisubstrate failure; ASTM C882
 
Processing PropertiesOriginal ValueComments
Dry Time <= 2.00 hour
Shelf Life 24.0 Month
@Temperature 5.00 - 25.0 °C
in original unopened cartridge
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIKA905 / 209812

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.