MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ashley Polymers Ashlene® 935 Nylon 11
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Unreinforced

Material Notes: An unplasticized Nylon 11 for extrusion applications.

Data provided by the manufacturer

Key Words: Polyamide 11; Ashley Polymers, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Water Absorption 0.30 %ASTM D570
Moisture Absorption at Equilibrium 1.1 %65% RH; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Tensile Strength, Ultimate 66.0 MPaATSM D638
Elongation at Break 290 %ASTM D638
Flexural Modulus 1.10 GPaASTM D790
Izod Impact, Notched 0.750 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 186 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 150 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 316 Cast Stainless Steel, SUS316 Hot Formed
Ashley Polymers Ashlene® T940H Nylon 11
Arkema Rilsan® BSR 30 PA11-CF30
Arkema Rilsan® BZM 30 O TL PA11-GF30
Permabond 935 Cyanoacrylate

PNAB80 / 54505

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.