MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chemours Krytox™ PRO PFPE Additive for Polymers
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fluoroguard™ PRO is a colorless, odorless, nonflammable, and chemically inert polymer processing additive based on fluorinated synthetic oil (perfluoropolyether). It has excellent color and UV/thermal stability. Added to plastics and elastomers, it improves processing characteristics and properties of polymer compounds. Fluoroguard™ PRO internally lubricates to improve flow properties, process ability, throughput, uniform mixing of ingredients, product gloss, surface quality, and offers other advantages over competitive process aids. Fluoroguard™ PRO oil has a boiling point of about 278 °C (532 °F).

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.90 g/cc
@Temperature 23.0 °C
Viscosity Measure 7.0 cSt
@Temperature 38.0 °C
Molecular Weight 1375 g/mol
Surface Tension 18 dynes/cm
@Temperature 26.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point 278 °C
Pour Point <= -70.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.30nD25
 
Descriptive Properties
AppearanceClear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDUPJ861 / 254050

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.