MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Outokumpu 904L High Performance Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Pressure Vessel Steel; Stainless Steel

Material Notes:

Applications:

  • Process equipment in chemical industry
  • Bleaching equipment in the pulp and paper industry
  • Flue-gas cleaning
  • Desalination
  • Seawater handling
  • Heat exchangers

Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.4539; ASTM 904L
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell >= 180Hot rolled plate/Hot rolled strip/Cold rolled strip; EN 10003-1
Tensile Strength, Ultimate 600 MPaOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 440 MPa
@Temperature 300 °C
EN min.; EN 10002-5
 460 MPa
@Temperature 200 °C
EN min.; EN 10002-5
 500 MPa
@Temperature 100 °C
EN min.; EN 10002-5
Tensile Strength, Yield 220 MPa
@Strain 0.2 %
EN min., RT; EN 10002-1
 260 MPa
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 300 MPa
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 125 MPa
@Strain 0.2 %,
Temperature 400 °C
EN min.; EN 10002-5
 145 MPa
@Strain 0.2 %,
Temperature 300 °C
EN min.; EN 10002-5
 155 MPa
@Strain 1 %,
Temperature 400 °C
EN min.; EN 10002-5
 175 MPa
@Strain 1 %,
Temperature 300 °C
EN min.; EN 10002-5
 175 MPa
@Strain 0.2 %,
Temperature 200 °C
EN min.; EN 10002-5
 205 MPa
@Strain 0.2 %,
Temperature 100 °C
EN min.; EN 10002-5
 205 MPa
@Strain 1 %,
Temperature 200 °C
EN min.; EN 10002-5
 235 MPa
@Strain 1 %,
Temperature 100 °C
EN min.; EN 10002-5
Elongation at Break 50 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Modulus of Elasticity 195 GPaRT
 166 GPa
@Temperature 400 °C
Poissons Ratio 0.30RT
Shear Modulus 75.0 GPacalculated
Impact Test >= 60.0 JHot rolled plate/Hot rolled strip/Cold rolled strip; EN 10045-1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000100 ohm-cmRT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.8 µm/m-°C
@Temperature 100 °C
 16.9 µm/m-°C
@Temperature 400 °C
Specific Heat Capacity 0.450 J/g-°CRT
Thermal Conductivity 12.0 W/m-KRT
 18.0 W/m-K
@Temperature 400 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1080 - 1160 °CSolution Annealing
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.010 %
Chromium, Cr 20 %
Copper, Cu 1.5 %
Iron, Fe 49.19 %
Molybdenum, Mo 4.3 %
Nickel, Ni 25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 2014-T6; 2014-T651
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904)
AISI Type 304L Stainless Steel
Outokumpu 2205 Duplex Stainless Steel

NOUTOK32 / 18747

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.