MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Envalior Arnite® TV4 261 SF PBT-GF30 FR(17)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: 30% Glass Reinforced, Flame Retardant, High Flow

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Water Absorption 0.30 %Sim. To ISO 62
Moisture Absorption 0.150 %Sim. To ISO 62
Viscosity 9000 cP
@Shear Rate 100000 1/s,
Temperature 270 °C
 10000 cP
@Shear Rate 100000 1/s,
Temperature 250 °C
 20000 cP
@Shear Rate 100000 1/s,
Temperature 230 °C
 1.00e+6 cP
@Shear Rate 1 1/s,
Temperature 270 °C
 2.00e+6 cP
@Shear Rate 1 1/s,
Temperature 250 °C
 3.50e+6 cP
@Shear Rate 1 1/s,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 130 MPaISO 527-1/-2
Elongation at Break 2.5 %ISO 527-1/-2
Tensile Modulus 11.0 GPaISO 527-1/-2
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 28.0 kV/mmIEC 60243-1
Dissipation Factor 0.0025
@Frequency 100 Hz
IEC 60250
 0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 300 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°CISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-1/-2
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 0.750 mm
IEC 60695-11-10
Glow Wire Flammability Index 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Arnite® TV4 264 SN PBT-GF30 FR(17)
Envalior Arnite® TV6 241 SN PBT-GF20 FR(17)
Envalior Arnite® TV4 261 PBT-GF30, 30% Glass Filled
Envalior Arnite® TV4 260 SXF PBT-GF30 FR(17)
Envalior Arnite® TV4 261 KL PBT-GF30

PDSM9773 / 161394

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.