MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Low Density (LDPE)

Material Notes: The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Since it presents gains in resistance in the weld region, this product meets the requirements of the cutting and welding line and/or of the automatic or semi-automatic packaging, contributing to the reduction of losses due to sacks breaking. The Trithene® TX 4003 resin presents excellent performance on conventional extruders for LDPE, ensuring thermal stability during the processing and allowing the production of films with good thickness uniformity. The components that form the product Trithene® TX 4003 complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Technical films for high resistance industrial packages and plastic tarps for various uses such as for covering structures and sheds, films for waterproofing, etc. Industrial bags, bags for packaging with greater mechanical resistance as well as against perforation and impact.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Petroquimica Triunfo has been acquired by Braskem.

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/ccASTM D1505
Thickness 50.0 microns
Melt Index of Compound 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 380 %ASTM D882
Film Elongation at Break, TD 765 %ASTM D882
Secant Modulus, MD 0.120 GPa5%; ASTM D882
Secant Modulus, TD 0.130 GPa5%; ASTM D882
Coefficient of Friction, Dynamic 0.50ASTM D1894
Elmendorf Tear Strength, MD 2.80 g/micronASTM D1922
Elmendorf Tear Strength, TD 2.60 g/micronASTM D1922
Dart Drop Test 180 g(method A); ASTM D1709
Film Tensile Strength at Break, MD 31.0 MPaASTM D882
Film Tensile Strength at Break, TD 36.0 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 16 %ASTM D1003
Gloss 63 %@ 60° Gardner; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 195 °CPlasticizing Zone
 200 - 210 °CMixture Zone
Feed Temperature 170 - 185 °C
Adapter Temperature 210 - 225 °C
Die Opening 0.0800 - 0.170 cm
Blow-up Ratio (BUR) 3.0Recommended
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Proportion LLDPE %22.5PTN-570-Q

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDAX107 / 29532

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.