MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Product Description: Mylar® OWF2 is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. Mylar® OWF2 has a thicker heat sealable layer than Mylar® OWF. This film is suitable for use in contact with food.

Approvals: FDA Food Contact Status - All gauges of Mylar® OWF2 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® OWF2 can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/cc
Thickness 0.600 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 100 %ASTM D882A
Film Elongation at Break, TD 90 %ASTM D882A
Coefficient of Friction, Dynamic 0.50A-B; ASTM D1894
Coefficient of Friction, Static 0.60ASTM D1894
Film Tensile Strength at Break, MD 25000 psiASTM D882A
Film Tensile Strength at Break, TD 27000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.17 J/g-°CTypical Mylar®
Melting Point 254 °CTypical Mylar® via DSC
Maximum Service Temperature, Air 250 °F
Shrinkage, MD 1.25 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD 0.30 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Haze 3.5 %ASTM D1003
Transmission, Visible 88.6 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)5 cc/100 in2O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal)33000 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge
DuPont Teijin Films Mylar® MO21 Polyester Film, 750 Gauge
DuPont Teijin Films Mylar® P25T Polyester Film, 50 Gauge
DuPont Teijin Films Mylar® P25 Polyester Film, 50 Gauge
DuPont Teijin Films Mylar® OWF Polyester Film, 48 Gauge

PDTZ9391 / 139711

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.