MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Ceramite® CSR Refractory
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Ceramite® CSA and CSR series are precast refractory materials based on silicon carbide. Used in areas of heavy wear in the aluminium industry, they have high abrasion resistance and high thermal conductivity. Different aggregates in each formulation determine the properties for each product. Ceramite CSA and CSR series are high performance refractories for high temperature applications.

Benefits:

  • Good strength
  • Good wear resistance
  • Good chemical resistance
  • High thermal conductivity
  • High thermal shock resistance
  • Alkali resistance

Information provided by Pyrotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
@Temperature 600 °C
 2.70 g/cc
@Temperature 20.0 °C
Grain Size <= 3000 µm
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0130 GPa
@Temperature 850 °C
Cold
 0.0140 GPa
@Temperature 600 °C
Cold
 0.0160 GPa
@Temperature 1000 °C
Cold
 0.0190 GPa
@Temperature 20.0 °C
Cold
 0.0250 GPa
@Temperature 1000 °C
Hot
Compressive Strength 112 MPa
@Temperature 850 °C
Cold
 115 MPa
@Temperature 1000 °C
Cold
 161 MPa
@Temperature 20.0 °C
Cold
 181 MPa
@Temperature 600 °C
Cold
Abrasion 0.80
@Temperature 20.0 °C
[cm^3]
 0.80
@Temperature 600 °C
[cm^3]
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 6.60 W/m-K
@Temperature 600 °C
 7.90 W/m-K
@Temperature 300 °C
Maximum Service Temperature, Air 1000 °C
Shrinkage -0.400 %
@Temperature 20.0 - 850 °C
 
Descriptive Properties
Permanent Linear Change-0.27%20-850°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Ceramite® AFA Refractory
Pyrotek Ceramite® T-D Dry Sprayable Gunite Refractory
Polynorbornene Rubber (PNR)
Polychloroprene Rubber (CR)
Polybutadiene Rubber (BR)

CPYRO515 / 199537

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.