MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay MIRANOL® H2M CONC Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: MIRANOL H2M CONC is a mild amphoteric surfactant derived from lauric acid. High foaming in greasy soils. Provides reduction in irritation in combination with anionics.

I.N.C.I. Name: DISODIUM LAUROAMPHODIACETATE

CAS: 68608-66-2,

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRANOL H2M CONC is a mild amphoteric surfactant derived from lauric acid. High foaming in greasy soils. Provides reduction in irritation in combination with anionics.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 49 - 51 %Moisture Balance; RP-0536
pH 8.0 - 8.5
@Temperature 30.0 °C
20% Solution; RP-0420
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
CompositionActive>37%, =%Solids-%Sodium Chloride
 Diamide<0.5%
 Sodium Chloride11.2-12.2, RP-0097

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Belsil® PDM 20 Trimethylsiloxyphenyl Dimethicone
Wacker Belsil® DPM 1000 Trimethylsiloxyphenyl Dimethicone
ExxonMobil Neo Decanoic Acid, Technical Grade
ExxonMobil Neo Decanoic Acid, Prime Grade
ExxonMobil ExxonMobil™ Nonene LSAT Higher Olefin

WRHOD258 / 137489

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.