MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® 2355-2 FEP Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® 2355-2 is manufactured from clear FEP (fluorinated ethylene propylene) film with pressure-sensitive, high-temperature silicone adhesive.

Features/Benefits: Both CHR® 2355-2 tape is very durable and versatile products. The FEP backing offers excellent high temperature resistance and they offer the highest electrical strength in volts per mm. FEP backing is chemically inert, thin and conformable. The tape construction is weather resistant, stable and non-toxic.

Applications: CHR® 2355-2 tape is often used for coil and transformer insulation. Due to its transparency, these tapes are useful for “see through” identification on wire harnesses.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 275 %
Tear Strength 8.00 pliInitial Tear Strength
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 9000 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -100 °F
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Nextel™ BP-18 Woven Tape 312 (5.1 cm)
3M Nextel™ BP-18 Woven Tape 312 (3.8 cm)
3M Nextel™ BP-18 Woven Tape 312 (2.5 cm)
3M Nextel™ AP-18 Woven Tape 312 (5.1 cm)
3M Nextel™ AP-18 Woven Tape 312 (3.8 cm)

PSTGQZ288 / 68802

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.