MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Aperam Supera 36 Cold Rolled Strip
Categories: Metal; Ferrous Metal

Material Notes: SUPRA 36 is an iron-nickel soft magnetic alloys with high permeability and with good resistivity. Main applications are clock motors parts, CTR gun grids.

International standards: DIN 17405 - IEC 404 - JIS C 2531

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 130Annealed
 230Hard Temper
Tensile Strength 480 MPaAnnealed
 700 MPaHard Temper
Tensile Strength, Yield 480 MPaAnnealed
 700 MPaHard Temper
Elongation at Break 3.0 %Hard Temper
 30 %Annealed
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0000075 ohm-cm
Magnetic Permeability 7000
@Thickness 0.350 mm
AC
 <= 30000
@Thickness 0.350 mm
DC
Magnetic Coercive Force, Hc 0.075 Oe
@Thickness 0.350 mm
Magnetic Saturation Flux Density, Bmax 13000 Gauss
@Thickness 0.350 mm
DC, Saturation Induction
 13000 Gauss
@Thickness 0.350 mm
AC, Saturation Induction
Curie Temperature 230 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.00 µm/m-°C
Specific Heat Capacity 0.500 J/g-°C
Thermal Conductivity 10.5 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 64 %
Nickel, Ni 36 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter Super Invar 32-5
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C)
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018
CeramTec GRADE A LAVA Machinable Ceramic
ATVS, AFNOR 25NCTDV25 Superalloy

NPERA012 / 194801

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.