Symbol according to ISO 1043/1: PC+ABS Similar to KOBLEND PCA 447 with improved fluidity and release, suitable to mould complex items. Unfilled. Suitable for Injection Molding. Supplied as pellets. ISO data. Information provided by Enichem Versalis is the Eni subsidiary containing the plastics and rubber businesses. |
Poly(Acrylonitrile Butadiene Styrene) + Polycarbonate |