MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Veradel® 3000MP Polyethersulfone (PESU)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Veradel® 3000MP is a high molecular weight polyethersulfone (PESU) homopolymer powder designed specifically for the fabrication of microporous and ultraporous filtration membranes, in both hollow fiber and flat sheet forms.

Veradel® 3000MP features high purity, excellent toughness and outstanding hydrolytic resistance. It also offers superior resistance to mineral acids and bases and good resistance to moderate concentrations of chlorine. All Veradel® PESU polymers may be sterilized using a variety of methods, including steam, gamma ray, e-beam and ethylene oxide.

Veradel® PESU polymers are also available in a range of lower molecular weight alternatives, from 3000MP down to the lowest molecular weight offering, 3600P. There is a direct correlation between molecular weight and solution viscosity.

Typical applications for which Veradel® 3000MP is suited include hemodialysis, drinking water purification, pretreatment for reverse osmosis plants, wastewater treatment, food and beverage processing, and a variety of other industrial and bioprocessing fluid filtration uses.

Markets/Uses: Membranes / Membranes / Biomedical; Membranes / Membranes / Bioprocessing; Membranes / Membranes / Food and Beverage Processing; Membranes / Membranes / Hemodialysis; Membranes / Membranes / Industrial Process Separations; Membranes / Membranes / UF/MF Low Pressure Water Filtration; Membranes / Membranes / Waste Treatment; Membranes / Membranes / Water Purification

Applications: Filtration Media; Membranes

Features: Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; Food Contact Acceptable; Good Adhesion; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Molecular Weight; High Tensile Strength; Hydrolysis Resistant; Low Flow; Medium Rigidity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccASTM D792
Water Absorption 0.60 %
@Time 86400 sec
ASTM D570
Viscosity 1800 cPSolution Viscosity; ASTM D445
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 220 °CASTM E1356
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorTransparent - Slight Yellow
FormsPowder
ProcessingCast Film; Coating; Solution Processing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4583 / 280383

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.