Description: Specialty and super-high impact grades for a variety of applications such as refrigerator liners, consumer electronics housings, recreation equipment and sporting goods, toys, office products, cosmetics and personal care products, building and construction, housewares, and furniture and furnishings. Information provided by BASF. Ineos Styrenics purchased this product line from BASF in 2005. |