MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Cosmic Plastics 306 Orlon Filled Diallyl Iso-Phthalate Molding Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP)

Material Notes: Description: Cosmic 306 is an orlon filled, general purpose diallyl ortho phthalate molding compound which is supplied in a flake form.

Features: It has excellent electrical properties and is unaffected by prolonged exposure to elevated temperature and 100% humidity. It is also resistant to solvents, acids, and alkalies.

Applications: Switches, terminals, insulators, cups, cases or other applications requiring strength and chemical or moisture resistance. Also useful for encapsulation of electrical and electronic components.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/cc
Bulk Factor 6.0
Water Absorption 0.35 %
@Temperature 50.0 °C,
Time 173000 sec
Linear Mold Shrinkage 0.0070 - 0.0090 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3600 - 5000 psi
Flexural Strength 8000 - 12500 psi
Compressive Strength 18000 - 30000 psi
Izod Impact, Notched 0.600 - 3.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cm
 1.00e+10 ohm-cm
@Temperature 70.0 °C,
Time 2.59e+6 sec
100% RH
Surface Resistance >= 1.00e+16 ohm
 1.00e+10 ohm
@Temperature 70.0 °C,
Time 2.59e+6 sec
100% RH
Dielectric Constant 3.1
@Frequency 1e+6 Hz
Dry
 3.2
@Frequency 1000 Hz
Dry
 3.3
@Frequency 1e+6 Hz
Wet
 3.4
@Frequency 1000 Hz
Wet
Dielectric Strength 340 V/milWet, step by step
 360 V/milDry, step by step
Dielectric Breakdown 50 VWet, step by step
 62 VDry, step by step
Dissipation Factor 0.013
@Frequency 1e+6 Hz
Dry
 0.015
@Frequency 1e+6 Hz
Wet
 0.020
@Frequency 1000 Hz
Dry
 0.022
@Frequency 1000 Hz
Wet
Arc Resistance 125 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 42.0 µm/m-°C
@Temperature -40.0 - 100 °C
Heat Distortion Temperature 260 °C
 
Processing PropertiesOriginal ValueComments
Mold Temperature 135 - 190 °C
 
Descriptive Properties
Dimensional Stability<0.07%
MIL-M-14SDI-5ASTM D5948-96
Molding Pressure500-8000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite RX® 643 Phenolic Resole Compound
Sumitomo Bakelite RX® 1310 Diallyl Ortho-Phthalate Molding Compound
Sumitomo Bakelite RX® 647 Phenolic Resole Compound
Cosmic Plastics K61/6230 Long Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound
Cosmic Plastics K43/6260 Mineral Filled Diallyl Iso-Phthalate Molding Compound

PCOSM002 / 190784

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.