MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Vacupor® TS-B2-S Porextherm
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Vacupor® TS-B2-S is a microporous inorganic oxide insulation material which has an extremely low thermal conductivity coefficient. The main constituent is fumed silica, the other components are opacifiers for minimizing infrared radiation, and fiber filaments as reinforcing fillers. Vacupor® TS-B2-S is approved by DIBT under the certification number Z-23.11-1662.The approval is valid for construction applications DAD, DAA, DZ, DI, DEO, WAB, WAA, WH, WTR and WI according to standard DIN 4108-10, and prefabricated façade panels with insulated glass character. Vacupor® TS-B2-S conforms to building material class E (B2). The test of behavior in case of fire according DIN 4102-1, May 1998, building material class B2; test certificate no. H.3-145/07 and H.3-146/07, was issued by the Forschungsinstitut für ärmeschutz e.V. München. The core material of Vacupor® TS-B2-S is not flammable and is classified A1 according to DIN ISO EN 13501-1. Vacupor® TS-B2-S is heat sealed in a multilayer vacuum metalised film. The very low internal pressure and the microporous panel core enable it to reach extremely low thermal conductivity values.

Application: Vacupor® TS-B2-S was specially developed for applications in the building and construction industry where an approval by the building authorities is required. The low density and IR opacifiers contained in these grades greatly reduce the thermal conductivity of Vacupor® TS-B2-S Systems. Due to the single- or double-sided coverage with a sound absorption recycling plastic board, Vacupor® TS-B2-S is particularly suitable for all kinds of plane linings. The fixing of the insulation is much easier, and the VIPs can be installed without any damage being caused. The fixing of the insulation is substantially facilitated, through the possibility of bonding with commercial solvent free adhesives. Vacupor® TS-B2-S is used as insulation material in the following applications: Reveal insulation, Insulation of basement ceilings, Insulation of roller shutter casings, Insulation of internal floors.

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.170 - 0.210 g/ccDepending on board thickness.
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 1.00 MPaat 210 kg/m3
 1.50 MPaat 230 kg/m3
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.00500 W/m-K
 0.00700 W/m-Krated value. According to DIBt general approval no. Z-23.11-16.
 <= 0.0190 W/m-Kat ambient pressure.
 0.00400 W/m-K
@Temperature 20.0 °C
 0.00363 W/m-K
@Pressure 1.00e-7 MPa
 0.00366 W/m-K
@Pressure 0.0000100 MPa
 0.00375 W/m-K
@Pressure 0.000100 MPa
 0.00425 W/m-K
@Pressure 0.00100 MPa
 0.00870 W/m-K
@Pressure 0.0150 MPa
Maximum Service Temperature, Air <= 120 °CThe limits are fixed by the barrier film; durable maximum temperature is at 80°C; short time maximum at 120°C for approximately 30 minutes.
Minimum Service Temperature, Air >= -50.0 °C
 
Descriptive Properties
Colorsilver/grey
Compression Behavior (%)10at 1 bar, 160kg/m3
 10at 3 bar, 230 kg/m3
 15at 2 bar, 160 kg/m3
 20at 3 bar, 160 kg/m3
 5at 1 bar, 230kg/m3
 8at 2 bar, 230 kg/m3
Sound Absorption Rate (ΔLW)18with glue flags on, dB
 40with glue carpet on, dB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Crystex Composites Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite

CMORF6129 / 202913

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.