MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® OM-13970 XRD1 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene OM-13970 XRD1 is a high performance thermoplastic elastomer, available in NAT and colors, designed for a variety of personal care consumer product applications requiring a soft, rubber-like feel, including toothbrush articles. Monprene OM-13970 XRD1 is a medium hardness, medium density, UV stabilized grade that complies with various US FDA and European regulations and directives for food contact and is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Filled; Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; High Elasticity; Medium Hardness; Lubricated; Medium Density; Medium Flow; UV Stabilized

Uses: Consumer Applications; Cosmetic Packaging; Food Containers; Food Packaging; Food Services Applications; Gaskets; Handles; Kitchenware; Lids; Non-specific Food Applications; Rubber Replacement; Toothbrush Handles; Toys

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 5.00 sec
ISO 868
 72
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1200 psiISO 37
Tensile Stress at Strain 334 psi
@Strain 100 %
ISO 37
 348 psi
@Strain 300 %
ISO 37
Elongation at Break 700 %ISO 37
Compression Set 34 %
@Temperature 22.8 °C,
Time 79200 sec
Method B; ISO 815
 55 %
@Temperature 70.0 °C,
Time 79200 sec
Method B; ISO 815
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 248 - 320 °F
Middle Barrel Temperature 320 - 446 °F
Front Barrel Temperature 356 - 446 °F
Nozzle Temperature 356 - 446 °F
Melt Temperature 356 - 446 °F
Mold Temperature 59.0 - 122 °F
Back Pressure 72.5 - 218 psi
Cushion 0.118 - 0.787 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0914 / 237405

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.