Desmoderm Finish WX is a one-component polyurethane based on an aliphatic diisocyanate. Uses: Solutions of Desmoderm Finish WX are suitable for use as finishes applied by the transfer and direct coating processes, especially in the manufacture of technical articles required to have a long service life. Information provided by Covestro |