MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Persian Gulf Polymer PP-EP548R Block Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: EP548R is a nucleated, antistatic formulated, high fluidity heterophasic copolymer used for thinwalled injection molding. Items made with "EP548R" exhibit high stiffness. Relatively good impact resistance and excellent antistatic properties. Due to its excellent moldability and short cycle items, "EP548R" allows high productivity rates. The finished items show good mechanical properties, high dimensional stability." EP548R" is very well suited for the production of thin walled articles or articles with long flow paths such as flower pots, containers, housewares, filters, filters housings and appliance components." EP548R" is suitable for food contact. Processing Method: Injection molding. Features: Good Impact strength, excellent antistatic properties, excellent moldability and short cycle time. Typical Applications: Housewares, filters, filters housing and appliance components, Sport, leisure and toys.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 21 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 98ASTM D785
Tensile Strength, Yield 27.0 MPaASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 1500 MPaASTM D790
Izod Impact, Notched 50.0 J/m
@Temperature -20.0 °C
ASTM D256
 85.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °CASTM D648
Vicat Softening Point 149 °C
@Load 1.02 kg
ASTM D1525
 
Descriptive Properties
Accelerated Oven Aging360 hrsIn air @ 150°C. ASTM D3012

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERSI981 / 250385

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.