MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones Elemax 2600 Silicone air and water-resistive barrier (AWB)
Categories: Polymer; Thermoset; Silicone

Material Notes: GE Elemax 2600 silicone air and water-resistive barrier (AWB) is a solvent free, fluid-applied, 100% silicone coating for AWB applications to coat and seal above-grade wall assemblies. Elemax 2600 silicone AWB coating provides long-term air and water protection from a variety of elements: temperature extremes, sunlight / UV radiation, rain and snow.

Features: Building Code Compliant, Seamless, Monolithic Air Barrier, Simple Installation, Reduced Energy Consumption, 100% Silicone Durability, UV Resistant, Self-sealing, Fire Characteristics, Elastomeric.

Applications: Seamless, breathable membrane, Simple One-coat Application, Primerless Adhesion, Extended Temperature Range, Rain Ready, Fast Cure, Application to Various Substrates, Silicone Compatibility, Clean Air GOLD.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 90 %Modified ASTM D2697
Volatile Organic Compounds (VOC) Content <= 24 g/lEPA Method 24
Viscosity 25000 cPASTM D2196, Method A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1.41 MPaSample prepared per ASTM D2370; ASTM D412
Elongation at Break 542 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 0.000 - 150 °FApplication Temperature
Cure Time 24.0 - 48.0 hour
 
Descriptive Properties
Air Permeance (cfm/ft2)4E-05ASTM E2178. Tested at 1.57 psf at 17 mils DFT
AppearancePourable liquid
Assembly Air Leakage0.0002 cfm/ft2ASTM E2357. tested at 1.57 psf at 17mils DFT
ColorBlack
 Gray, whiteUpon request
Crack Bridging Ability (1/16")passASTM C1305
Mildew Resistance0- no growthASTM D5590
Pull of Strength126 psiASTM D4541. Concrete
 44 psiASTM D4541. fiberglass mat faced gypsum sheathing
Resistance to Wind Driven RainResistance to Wind Driven Rain Pass: No visual leaks or moisture weight gain observed after 24 hrs @ 26 psf.ASTM D6904
Self Sealability around nailsPassASTM D1970
UV & Weathering ResistanceNo degradation after 5000 hoursASTM G154
Water PenetrationNo water penetration observed after 15 minutes @ 62.5 psf .ASTM D331
Water Vapor Permeance10.2 perms@ 17 mils DFT. ASTM E96 Procedure B (Water Method)
 7.9 perms@ 17 mils DFT. ASTM E96 Procedure A (Desiccant Method)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9907 / 265716

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.