MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Röchling Durostone® UPM S16 Reinforced Polyester Sheet
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Durostone® UPM S16 is a fiber-reinforced plastic for applications that provide an increased mechanical strength as a requirement. Flammability IEC 60707 is FVO >5 mm.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.87 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 100 MPaParallel; ISO 527
Modulus of Elasticity 13.0 GPaPerpendicular; ISO 178
Flexural Strength 200 MPaPerpendicular; ISO 178
Compressive Strength 250 MPaPerpendicular; ISO 604
Izod Impact, Notched (ISO) 80.0 kJ/m²Parallel; ISO 179
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 12.0 kV/mm
@Temperature 90.0 °C
Perpendicular; EC 60243
 50.0 kV/in
@Temperature 90.0 °C
Parallel; IEC 60243
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 - 30.0 µm/m-°C
Thermal Conductivity 0.300 W/m-KISO 8302
Maximum Service Temperature, Air 155 °CThermal Endurance; IEC 60216
Flammability, UL94 V-0
@Thickness >=1.00 mm
 
Descriptive Properties
Colorgrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROCH9076 / 232779

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.