MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Nouryon Perkadox PD-50S-PS Crosslinking-row Di(2,4-dichlorobenzoyl) peroxide
Categories: Other Engineering Material

Material Notes: Diacyl peroxide, 50% active ingredient in silicone oil and silica, in paste form for ease of dispersion. The most common organic peroxide used in silicone rubber, particularly injection-molded rubber articles.

CAS number: 133-14-2

EINECS/ELINCS No.: 205-094-9

Applications: Perkadox PD-50S-ps is mainly used for the crosslinking of silicone rubbers. With Perkadox PD-50S-ps silicone rubber compounds can be cured without external pressure (hot air and/or IR vulcanization).

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/cc
Molecular Weight 380 g/mol
Storage Temperature <= 30.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 60.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 1.5 %
 
Descriptive Properties
AppearanceOff-white homogeneous paste
Assay49.0-51.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY827 / 286350

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.