MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 1099 X 87257 B Polybutylene Terephthalate (PBT) Carbon Nanotube - ESD Protection - Static Dissipative  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D 792
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8500 psiASTM D 638
Elongation at Break 3.0 - 6.0 %ASTM D 638
Tensile Modulus 500000 psiASTM D 638
Flexural Strength 15000 psiASTM D 790
Flexural Modulus 500000 psiASTM D 790
Izod Impact, Notched 0.500 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 9.00 ft-lb/in
@Thickness 3.17 mm
ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10 - 10000 ohm-cmASTM D 257
Surface Resistance 1000 - 1.00e+6 ohmESD STM11.11
Surface Resistivity per Square 10000 - 1.00e+7 ohmASTM D 257; ESD 11.11
Static Decay <= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 460 - 520 °F
Mold Temperature 175 - 225 °F
Drying Temperature 250 °F4 hrs
Moisture Content 0.030 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 399 X 143507 Polycarbonate (PC); ESD Protection - Static Dissipative - Flame Retardant
RTP Company RTP 399 X 115069 D Polycarbonate (PC), Carbon Nanotube - Electrically Conductive - ESD Protection
RTP Company RTP 382 HEC FR  Polycarbonate (PC) Nickel-Coated Carbon Fiber 15% - Flame Retardant - EMI/ESD
RTP Company RTP 3399 X 117884 F Polyvinylidene Fluoride (PVDF), Carbon Nanotube - ESD Protection - Static Dissipative
RTP Company RTP 2583 C HEC  Polycarbonate/ABS Alloy (PC/ABS) Nickel-Coated Carbon Fiber 20% - EMI/ESD

PQZZ3184 / 61425

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.