Description: Special PA 50% glass fibre reinforced, high flow injection moulding grade. Heat stabilized. Drinking water and food contact. Black colour. General purpose metal replacement product with good resistance to hydrolysis, enhanced mechanical properties after moisture pick-up. Specifically intended for use in applications in civil and industrial water management as well as appliances and consumer goods. Suitable for parts requiring very high stiffness and high mechanical resistance along with high surface quality and superior gloss. Processing: Injection Molding Delivery Form: Granules Additives: Release agent Special Characteristics: Heat stabilized or stable to heat, Improved Fluiditiy, Hydrolysis Resistance, Food Contact, High Surface Aspect Industries: Consumer Industry Goods, Water Management Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa Information provided by Radici Group |