MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Shell Carilon® D26VM100 Polyketone, High-Flow Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26VM100 is a high-flow injection molding grade with mechanical properties which classify it as an engineering thermoplastic. This grade exhibits very good processability, good impact resistance, high resilience and good creep performance. CARILON Polymer D26VM100 can also withstand short-term exposure to elevated temperatures. Moreover this polymer exhibits a high resistance to hydrocarbons, solvents, salt solutions, weak acids and weak bases. CARILON Polymer D26VM100 is a high-flow, low-viscosity polymer that should be considered for moldings with long flow paths or thin walls. This grade is very easy to process on standard injection molding equipment. Cycle times are generally short. Parts show good mold definition with glossy mar-resistant surfaces. CARILON Polymers' low moisture sensitivity means that no conditioning of parts before assembly or use is necessary.

Data provided by Shell Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.45 %24 hour immersion; ASTM D570
Moisture Absorption at Equilibrium 0.50 %at 50% RH; ASTM D570
Water Absorption at Saturation 2.2 %ASTM D570
Linear Mold Shrinkage, Flow 0.020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.021 cm/cmASTM D955
Melt Flow 60 g/10 min
@Load 2.16 kg,
Temperature 240 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Hardness, Shore D 77ISO 868
Tensile Strength, Ultimate 45.0 MPaASTM D638
Tensile Strength, Yield 60.0 MPaASTM D638
Elongation at Break >= 250 %ASTM D638
Elongation at Yield 20 %ASTM D638
Tensile Modulus 1.50 GPaASTM D638
Flexural Strength 59.0 MPaat 5% strain; ASTM D790
Flexural Modulus 1.50 GPaASTM D790
Izod Impact, Notched 0.950 J/cmASTM D256
Izod Impact, Unnotched NBASTM D256
Gardner Impact >= 45.0 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 ohm-cmASTM D257
Surface Resistance 1.00e+14 ohmASTM D257
Dielectric Constant 5.3
@Frequency 1e+6 Hz
ASTM D150
 6.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
@Thickness 1.60 mm
Short Term; ASTM D149
Dissipation Factor 0.010
@Frequency 1000 Hz
ASTM D150
 0.050
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 600 VUL746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°C
@Temperature 25.0 - 55.0 °C
ASTM E831
Melting Point 220 °C
Deflection Temperature at 0.46 MPa (66 psi) 203 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °CASTM D648
Flammability, UL94 HB
Oxygen Index 22 %ISO 4589

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
BASF Styroblend® PC 2065 Impact Grade Polystyrene Blend
Shell Carilon® DP P1000 Polyketone
Lehvoss LUVOCOM® 1105-8344/EM/GY PEEK unreinforced, easy flowing
Akro-Plastic Akrotek® PK-HM (4773) PK Dry

PCAR06 / 27915

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.