MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODAPON® UB-STD Surfactant
Categories: Fluid

Material Notes: Chemical Name: SODIUM LAUREL SULFATE

CAS: 68585-47-7

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAPON® UB-STD is a primary anionic surfactant for emulsion polymerization. RHODAPON© UB STD is used as a primary foaming and cleansing agent in shampoos, liquid soaps, and related cosmetic products. RHODAPON© UB STD has excellent detergency making it well suited for industrial and household cleaning applications as well.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 7.5 - 8.510% Solution; RP-0420
Viscosity <= 100 cPRP-0596
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Fe (Iron) <= 5.0 ppmO-Phenanthroline; RP-0277
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClean, Clear LiquidRP-0596
Cloud point<18°CRP-0123
Color<70Keltt, 50% Solution, RP-0139
CompositionActive29-30%, EQ. WT 305, RP-0033
 Free Oil<0.8%, RP-17303
 NaCL0.0015
 NaSO40.0065
 Sodium Chloride<0.25%, RP-0098
 Sodium Sulfate<1.0%, RP-0555
Critical Micelle Concentration (%)0
Foreign MatterFree of Foreign MatterRP-0636
HLB number40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODAFAC® RE-610 Surfactant
Solvay RHODAFAC® RA-600 E Surfactant
Solvay RHODAFAC® PE-510 Surfactant
Solvay RHODAFAC® PA32 Surfactant
Solvay RHODAFAC® MB Surfactant

WRHOD420 / 137651

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.