BETADAMP™ 32HT is a high temperature vibration damper that can be applied to the exterior of cast aluminum or steel engine valve, transmission, and crankcase (oil pan) covers or electro-coat substrates in paint shop on interior or exterior applications. BETADAMP™ 32HT has excellent thermal resistance. BETADAMP™ 32HT is epoxy base material containing no Poly Vinyl Chloride (PVC). Information provided by Dow |