LNP THERMOCOMP LCF62E compound is based on Polyetheretherketone (PEEK) resin containing 10% carbon fiber and 30% glass fiber. Added features of this grade include: Easy Molding, Electrically Conductive. Features: High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Electrically Conductive,Easy Molding,Structural Information provided by SABIC |