MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Redwood Plastics REDCO™ MD-OIL Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Redco™ Nylon MD-Oil filled is one of the most versatile standard grades of Redco™ Cast Nylon. Redco™ Nylon MD-Oil provides the same high compressive strength and load bearing properties of MD filled, with all the advantages of a liquid lubricant. Redco™ Nylon MD-Oil is especially suited for high load - low RPM applications, but is a superior replacement for MD in many heavy-duty friction generating applications.

Typical Applications: Pillow blocks, trunnion bearings, rope sheaves, pulleys, sprockets, slipper pads, dryer bushings, and custom components.

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/cc
Water Absorption 1.0 - 5.0 %Equilibrium
 0.20 - 0.50 %
@Time 86400 sec
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 10000 - 12000 psi
@Time 86400 sec
Elongation at Break 20 - 45 %
Tensile Modulus 350000 - 450000 psi
Flexural Strength 12500 - 15000 psi
Flexural Modulus 420000 psi
Compressive Strength 14500 psi10% Deflection
Coefficient of Friction 0.13 - 0.20Dry vs.Steel
Limiting Pressure Velocity 5000 psi-ft/min
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°C
Maximum Service Temperature, Air 250 °C
Minimum Service Temperature, Air 200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW035 / 296601

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.