MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow High Thermal Conductivity Silicon Nitride
Categories: Ceramic; Nitride

Material Notes: High Thermal Conductivity - much higher than typical silicon nitride. High fracture toughness. Surface roughness of Ra 0.02 µm achievable through polishing.

Used in Power module substrates; Various types of heat sinks; LED mounting substrates; High frequency circuit substrates.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 312 GPa
Flexural Strength 700 MPa
Poissons Ratio 0.29
Shear Modulus 121 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.00 µm/m-°C
@Temperature 25.0 - 800 °C
Thermal Conductivity 100 W/m-K

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Techical Ceramics Ekasic® S Silicon Nitride
3M Techical Ceramics Ekatherm® Silicon Nitride
Goodfellow Gas Pressure Sintered Silicon Nitride Si3N4
Goodfellow Hot Pressed Silicon Nitride Si3N4
Morgan Advanced Ceramics SSN Sintered Silicon Nitride Mac-SSNS

CGOODF248m / 197462

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.