MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® E42A NC010 PA66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Unreinforced High Viscosity Polyamide 66 Developed for Extrusion

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDAM; ISO 1183
Melt Density 1.01 g/cc
@Temperature >=263 °C
Water Absorption 8.5 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 2.70 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 300 cm³/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.014 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 52.0 MPa50% RH; ISO 527-1/-2
 86.0 MPaDAM; ISO 527-1/-2
Elongation at Break >= 50 %50% RH; ISO 527-1/-2
 >= 50 %DAM; ISO 527-1/-2
Elongation at Yield 5.0 %DAM; ISO 527-1/-2
 27 %50% RH; ISO 527-1/-2
Tensile Modulus 1200 MPa50% RH; ISO 527-1/-2
 3100 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.37DAM; ISO 527-1/-2
 0.4450%RH; ISO 527-1/-2
Izod Impact, Unnotched (ISO) 4.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 4.30 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 5.50 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 6.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cm50% RH; IEC 62631-3-1
 1.00e+13 ohm-cmDAM; IEC 62631-3-1
Dielectric Constant 3.6
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 4.2
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 4.3
@Frequency 100 Hz
DAM; IEC 62631-2-1
 10.3
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Dielectric Strength 30.5 kV/mmDAM; IEC 60243-1
Dissipation Factor 0.015
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.024
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.075
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 0.20
@Frequency 100 Hz
50% RH; IEC 62631-2-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CDAM; ISO 11359-1/-2
Specific Heat Capacity 2.79 J/g-°C
@Temperature >=263 °C
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature >=263 °C
Melt
Melting Point 263 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °CDAM; ISO 75-1/-2
Vicat Softening Point 244 °C50°C/h, 50N; ISO 306
Glass Transition Temp, Tg 70.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 0.810 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 28 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 275 - 290 °CExtrusion
 285 °CExtrusion Optimum
 290 °CInjection Optimum
 280 - 300 °CInjection
Mold Temperature 50.0 - 90.0 °CInjection
 70.0 °CInjection Optimum
Ejection Temperature 190 °CInjection
Drying Temperature 80.0 °CExtrusion
 80.0 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
 4.00 - 6.00 hourDehumidified Dryer; Extrusion
Moisture Content 0.050 %Injection
 0.060 %Extrusion
Hold Pressure 50.0 - 100 MPaInjection
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)4Injection
Max. screw tangential speed (m/s)0.4Injection
Part Marking CodePA66ISO 11469
ProcessingCasting
 Coatable
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
Regional AvailabilityEurope
 Near East/Africa
Resin IdentificationPA66ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 42A NC010 PA66
Envalior Durethan® A 30 S FN31 000000 Nylon 66 (PA66), Dry
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
Celanese Zytel® 70K20HSL NC010 PA66-RF20
Envalior Durethan® DP 2325 H3.0 000000 Nylon 66 (PA66), Dry

PDSX5390 / 198030

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.