MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
A. Schulman Lucent TPP-240 Polypropylene, 40% Talc Filled, Impact Modified
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Talc Filler

Material Notes: Melt Flow Adjustable for Application
Add "U" for UV Stabilized
Add "H" for Heat Stabilized

Information provided by Lucent Polymers, Inc. Lucent was acquired by A. Schulman in 2015.

Key Words: TPP, PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.010 cm/cm
@Thickness 3.17 mm
1/8" Section
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 27.59 MPaASTM D638
Elongation at Break >= 10 %ASTM D638
Flexural Strength 50.37 MPaASTM D790
Flexural Modulus 3241 MPaASTM D790
Izod Impact, Notched 80.1 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 79.44 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman TPP40AD61WH 40% Talc Filled, Heat Stabilized, Homopolymer Polypropylene
A. Schulman TPP40AC27NA 40% Talc Filled, Heat Stabilized, Homopolymer Polypropylene
A. Schulman Lucent TPP-340 Polypropylene, 40% Talc Filled, Impact Modified
A. Schulman Lucent TPP-140 Polypropylene, Homopolymer, 40% Talc Filled
A. Schulman TPP40AC52BK 40% Talc Filled, Heat Stabilized, Homopolymer Polypropylene

PLUCE100 / 90019

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.