Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ) and good light resistance. Vicat/B50 = 110°C Main application fields: business machines, electronic and electrical industry Unfilled. Suitable for Injection Molding. Supplied as pellets. ISO data. Information provided by Enichem Versalis is the Eni subsidiary containing the plastics and rubber businesses. |
Poly(Acrylonitrile Butadiene Styrene) + Polycarbonate |