MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay MTM® 55 Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: MTM55 is a controlled flow, 120°C (248°F) curing epoxy resin developed for autoclave, oven vacuum bag and press molding of components where exceptional surface quality is required. MTM55 exhibits enhanced toughness and is particularly suited to cosmetic applications and the sports good market.

Features & Benefits:

  • 60 days out life at 21°C (70°F)
  • 12 months storage at -18°C(0°F)
  • Supplied on a range of lightweight surface plies and a limited range of heavier reinforcements
  • Service temperature up to 90°C (194°F)
  • Good tack and drape characteristic
  • Exceptional surface quality
  • Enhanced toughness

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccCured resin, 1 hr at 120°C
Storage Temperature -18.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °C
Glass Transition Temp, Tg 119 °C1 hr at 120°C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Cast, Metal Filled
Overview of materials for Epoxy, Thermally Conductive
Hexcel® HexPly® F593 Epoxy Resin
Sulfur Hexafluoride, SF6
Permabond ET5401 Epoxy Resin

PCYTED148 / 180450

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.