Duplex stainless steel, UNS S32304 Sandvik SAF 2304TM is a duplex stainless steel (austenitic-ferritic) with a low carbon content. The material is characterized by the following properties: very good resistance to stress corrosion cracking.good resistance to general corrosion an pitting. high strength - approximately twice as high proof strength as austenitic stainless steels.physical properties that offer design advantages. ease of fabrication and good toughness.good weldability
Information provided by Sandvik UNS S32304; EN 1.4362 |