MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil EXACT™ 4011 Plastomer for Cast Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE

Material Notes: Ethylene based butene plastomer produced using ExxonMobil Chemical Exxpol technology. This resin is designed primarily for use in blends with polyolefins to improve the heat sealing performance and toughness in film applications.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.888 g/ccExxonMobil Method
Thickness 1.00 mil
Melt Flow 2.2 g/10 minExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 630 psi2% Offset; ASTM D882
Film Tensile Strength at Yield, TD 470 psi2% Offset; ASTM D882
Film Elongation at Break, MD 440 %ASTM D882
Film Elongation at Break, TD 820 %ASTM D882
Film Elongation at Yield, MD 14 %ASTM D882
Film Elongation at Yield, TD 10.7 %ASTM D882
Puncture Energy 54.9 in-lbExxonMobil Method
Elmendorf Tear Strength, MD 30.0 g/milASTM D1922
Elmendorf Tear Strength, TD 90.0 g/milASTM D1922
Dart Drop 120 g/milASTM D1709A
Film Tensile Strength at Break, MD 9400 psiASTM D882
Film Tensile Strength at Break, TD 6700 psiASTM D882
1% Secant Modulus, MD 5300 psiASTM D882
1% Secant Modulus, TD 5200 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 156 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 53.0 °CExxonMobil Method
Vicat Softening Point 133 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 0.50 %ASTM D1003
Gloss 89 %ASTM D2457
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 4150 Plastomer
ExxonMobil EXACT™ 4044 Plastomer for Extrusion Coating and Cast Film Applications
ExxonMobil EXACT™ 3131 Plastomer for Cast Film Applications
ExxonMobil EXACT™ 3125 Plastomer for Blown Film Applications

PEXB350 / 37655

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.